In flexible packaging, cast polypropylene (CPP) has quietly become the workhorse—snack pouches, bakery sleeves, flower wrap, retort laminations, the lot. And, to be honest, the market’s been buzzing: converters want cleaner optics, brands want tougher seals at lower temps, and sustainability teams want mono-material paths that actually run on existing lines. That’s where Cpp Film—especially from factories that control resin sourcing—earns its keep.
Cpp Film from LIYA is produced in Plastic Packing Park, Xiongxian, Baoding, Hebei province, China 071800. They source prime PP resins directly from PetroChina, Sinopec, Sabic, Equate, ExxonMobil, Dow Chemical, Total, and Borouge. That direct buy—no mystery blends—usually means tighter spec windows and, surprisingly often, better price stability.
| Property | Typical Value | Method |
|---|---|---|
| Thickness | 18–60 μm (custom up to 100 μm) | Micrometer |
| Density | ≈0.90 g/cm³ | ISO 1183 |
| Haze | ≤3–5% (clear grade) | ASTM D1003 |
| Tensile Strength (MD/TD) | 60–120 / 120–200 MPa | ASTM D882 |
| Elongation at Break | >350% MD / >200% TD | ASTM D882 |
| Coefficient of Friction | 0.20–0.40 (one/both sides) | ISO 8295 |
| Heat Seal Init. Temp | ≈105–120°C (seal layer) | Lab hot tack |
| Seal Strength | 8–18 N/15 mm | ASTM F88 |
| WVTR / OTR | ≈2–7 g/m²·day / ≈1000–2000 cc/m²·day | ASTM F1249 / D3985 |
Cpp Film shines in horizontal form-fill-seal bakery packs (low-temp seals, good stiffness), bouquet sleeves (clarity + tear), and as a heat-seal layer in PE/PA/AL laminates. Some electronics lines like its low static; others specify anti-fog for chilled produce. One QC manager told me, “We finally stopped fiddling with jaw temps at 3 a.m.”—that’s the seal window doing its job.
| Vendor | Resin Traceability | Optics | Lead Time | Customization |
|---|---|---|---|---|
| LIYA (China) | Direct from majors; lot-level COA | Low haze, high gloss | 2–4 weeks (typ.) | Slip/COF, AF, matte, corona, widths |
| Regional Converter A | Mixed sourcing | Moderate haze | 1–3 weeks | Standard SKUs |
| Import Aggregator B | Varies by batch | Inconsistent | 4–8 weeks | Limited |
Options include anti-fog, matte, pearlized, metalizable base, and treated/non-treated faces. Certifications frequently requested: ISO 9001/14001, food-contact conformity (e.g., U.S. FDA 21 CFR 177.1520; EU 10/2011) and RoHS/REACH declarations. Ask for migration and NIAS statements if you’re in retort or fatty-food applications.
A bakery in the Gulf swapped older BOPP/CPP laminate for a mono-CPP printable structure. Results after 60 days: seal temp down ≈10°C, jaw dwell cut 15%, pack clarity up (haze from 6.2% to 3.8%), and—this was unexpected—line stoppages for seals dropped by about a third. I guess when your film’s profile is consistent, operators stop babysitting the machine.
The trend is toward mono-material PE/PP where possible. Cpp Film is the enabling seal layer for PP-based recyclability while keeping the crisp look brands love. It’s not perfect—barrier is modest—but paired with coatings or metalization, it punches above its weight.